Hi,

I use Tmax chemical for TMAX films. For 120 format I take 100ml chemical + 400ml water. Develope time is 5 minutes 10 seconds in 26 degree Celcius.Before starting developer wash the film with normal filtered water which is 26 degree celcius.

I don't think you don't have to worry about temperature when you print,for muligrade paper 2 minutes in 1:2 diluted chemical in ilford bromophen paper developer.

I don't know about The "Photographers Formulary" in Montana packages alternate developers for TMAX films.

Thanks Mohammad Irfanul Islam Darkroom Section Drik Picture Library E-mail: darkroom@drik.net