Hi, I just wanted to clarify that all the process is being done in 20C. The water bath between the developer and fixer is also at 20C and it doesn't last longer than 1.5min I did try using Kodak Rapid Fixer which is contains hardener but no apparent difference. The negs do not look overdeveloped. The only slight difference in temperature is in the final bath with photoflo mixed with filtered water around 23C. I don't think that small variation would cause reticulation. I'm seriously considering using the TmaxCN from Kodak that can be processed in C41. I saw enlargements from it with almost no apparent grain. Herbet.