Response to Yellowing of photographs

from Ted Kaufman (writercrmp@aol.com)
I think you are hinting at the answer in your post. It sounds to me like the drymount press heat might have done something to the plastic coating. Do you recall the temperature setting you used? If you used regular drymount tissue, which I think requires 250 degrees, you might have overheated the plastic coating. I believe drymount tissue for RC requires only 180 degrees.