Hi, The following formula was posted here a month or two ago.(posted 8227 days ago)"Part A: 8g ascorbic acid + 0.8g metol / 500ml distilled water Part B: 6.8g sodium hydroxide + 24.4g borax / 500ml distilled water" Among other films, Delta 400, which I've never used, was suggested for this developer.
I'm wondering if you could share the experiences you all have with this developer and Delta 400, FP4, TX400 etc.
I currently use TX400 with Xtol or with HC-110 dil. "B".
I'd appreciate some input as to what the Vit. C developer does that is different.
Thanks! Howard