from N Dhananjay (ndhanu@umich.edu)
Are you referring to reticulation? It used to happen if the variation in temperature between developer and stop was high - a sort of crinkling of the emulsion. I've never tried it but I've heard it is quite difficult to do with modern emulsions. Try a big temperature difference and a strong acid stop (which is supposed to help). Good luck. DJ