I am currently developing TX (not TXP) in XTOL 1+2 at 5.5 minutes, 75 degrees, rotation speed 4, in a Jobo CPP2 processor. Does any body out there have times for same film in D76 1+1 (in a Jobo at 75~)? Thanks,