The little bit of Neopan 1600 that I've done in PMK was exposed at 800 and developed 10 minutes at 70F. I found I preferred the results of HP5+ exposed at 800 and developed in more "regular" developers, so haven't used the Neopan 1600 much.(posted 8339 days ago)